I'M MAKING FLUORINE (Patreon)
Content
...at least I'll try to...never seen this done before, so it's hard to say how easy it is, but it shouldn't be too bad in theory.
Today I received a very important package in the mail...a package containing this little contraption. It's made of half-inch-thick 316L stainless steel, 3D printed by JLCPCB, and it was designed for one purpose: producing the world's most dangerous element. I can't give an exact timeline of events, but here is the general plan going forward:
1. I need to first distill anhydrous hydrogen fluoride. I'll be using a solid steel retort and distilling into a dry-ice-cooled receiving vessel to condense everything. I'll probably make a video about this, since anhydrous HF is a pretty impressive chemical by itself, and I'll be using a few milliliters of it to make fluoroantimonic superacid.
2. Next, I'll need to dissolve potassium bifluoride in the anhydrous HF...hopefully this goes smoothly. There isn't much info on the process, so it could either solidify nicely or require melting to form the HF*KHF2 (melting point is around 70C).
3. Finally, I'll be performing electrolysis on the melted HF*KHF2 in the steel unit I designed, using graphite electrodes and a copper pipe to direct the fluorine flow. The cup shape underneath the lid should isolate the fluorine from the hydrogen and allow it to flow exclusively through the tube.
Some unknowns are:
1. How will the HF mingle with the KHF2? Will I have to add extra to dissolve everything and then allow the excess HF to evaporate until I get a solid that melts at 70C?
2. How easy will it be keeping things anhydrous? Will a little water kill everything, or will it be fine after it bakes out? I'll try to use weak oleum (100-105% sulfuric) to get dry HF, but idk...
3. Will the electrolysis actually work?? I mean, yes it 100% should, but I'm the first amatuer to try this in recent times, at least publicly. I've tried making sodium before via electrolysis, and even it has trouble forming...what if fluorine just keeps dissolving into the solution and HF boils out instead?
4. How will the steel passivate? This is the process that allows steel to be used with fluorine and HF, and it basically involves the outmost layer of metal being intentionally corroded. This forms a thin iron fluoride layer that cannot be corroded further. Will the steel/copper consume all of the fluorine as it's produced, or will it passivate like it should?
There's a lot to uncover about this process, but I fully intend to do so. Regarding safety, I feel like I am at least reasonably prepared. I have a full-body sleeved apron made of HF-resistant hydrophobic plastic, my full-face gas mask with HF-rated 3M cartridges, arm-length neoprene gloves (recommended for HF use), gloves to go beneath said gloves, and of course, my fume hood. I'll probably move the fume hood to my yard just to be extra safe, and maybe I'll even take it somewhere farther away...we'll see, I still need to figure it all out.
Just know that I am on track to make fluorine, and with luck, it'll be within the next few weeks! Until then, I have my "nitrite from curing salt" video coming out soon, and by the looks of it, Patrons will have almost a full week of early access.