It might be a few weeks before the next video is done...not because anything has gone wrong, it'll just take a while for me to actually do, film, and edit everything!

I was hoping to do a video on anhydrous HF and fluoroantimonic acid, but there have been a few complications. As it turns out, HF is kinda hard to make! Unlike hydrogen chloride, which can be easily generated by adding sulfuric acid to salt, the synthesis of hydrogen fluoride requires heating (the reaction of sulfuric acid with most fluoride salts is endothermic). I've tried to make it using my steel retort twice now, and both times I apparently couldn't get it hot enough. And during my second attempt, which got up to about 160C, the reaction mixture also overflowed into the collection vessel. So for now, I'm taking a break from HF...it's just too much of a pain to work with! In the future, if and when I reattempt, I'll be using a larger retort to avoid the boil-over issues, as well as heating everything to a higher temperature.

Now, onto fluorine. I have a hard time remembering everything I've shared, and some of you are new supporters, so I'll try to cover everything here: I'm making fluorine gas. JLCPCB reached out a few months ago looking to sponsor a video, and since they offer metal 3D printing, I jumped at the opportunity and had them print me a stainless steel electrolysis cell. Around the same time, I order a set of graphite electrodes and a pound of potassium bifluoride (KHF2).

At first, I planned to dissolve the KHF2 in anhydrous HF (the typical industry practice) and simply run with what I had. However, my HF synthesis failed, so I looked for alternatives. Fortunately, this search lead me to the paper I've attached to this post (read it if you'd like), which told me that regular KHF2 works fine! As far as I can tell, the HF just helps lower its melting point (70C instead of 230C).

This paper also brought a few things to my attention...mainly two things that could potentially hinder my electrolysis, which are water and silicon. Water is kinda obvious: it will simply react with the fluorine, creating HF, oxygen difluoride, hydrogen peroxide, etc. The paper's solution was to bake the KHF2 at 130C for 48 hours. I tried starting that process yesterday, but my cheap $20 oven lacks proper temperature control, so I found it idling at 180C and had to shut it down (even though I had tested it at 130C several times...I guess the cheap thermal switch weakens after hours of continuous service). Above 130C, small amounts of HF can be lost, which isn't desirable. I purchased a digital PID temperature controller, and when it arrives on Saturday, I will hook it up to my oven and continue the bakeout.

Silicon is the other thing that can mess up the electrolysis. According to the paper, even a few percent of silicon in the KHF2 or graphite electrodes can cause a glassy layer to build up on the electrodes' surface, inhibiting further electrolysis. The KHF2 quality is somewhat hard to ensure and cannot be easily improved at home, but it was bought from a reputable company (GFS Chemicals through Chemsavers), and listed as at least 98% pure. In contrast, the graphite quality is REALLY hard to verify (it was bought on Amazon as "99.9%"), but it is potentially fixable at home! I spent yesterday refining my electrodes, using a bath of molten sodium hydroxide to leach out any silicon-based impurities. This was followed by several washings, bakeouts, and even electrolysis runs in dilute HCl (to pull out any residual NaOH) and sodium fluoride. The sodium fluoride electrolysis doesn't produce fluorine, but it does create HF and active fluoride ions around the anode, which I figured might be able to strip out any remaining silicon.

It's hard to say how things will actually go with the fluorine synthesis. In theory, everything should be fine: I'm using the correct materials, applying the same power, and even running the process in a custom steel vessel! But...unknowns exist. What if the fluorine doesn't bubble up through the cell like it's supposed to and instead mingles with the hydrogen? What if there is silicon in my KHF2 or graphite? Could I still get at least some fluorine in that case? Will I properly bake out the KHF2? What if I overcook it and HF is lost? What if the fluorine reacts with everything before it even exits the electrolysis setup? DO I EVEN POST THE VIDEO IF I FAIL???

(I kinda have to, since JLCPCB sponsored it, but that'd suck for a 100K special)

For now, we'll just have to wait and see what happens!