BRIEF UPDATE: I FAILED (Patreon)
Content
I spent Saturday trying to get at least one puff of fluorine, but came up short. No more retries until Christmas break...ngl, this kinda sucks.
I bought some stainless steel measuring cups to use as vessels for my molten potassium bifluoride, but upon heating the bifluoride in one, I noticed some bubbling. Apparently, at 250C, KHF2 attacks steel. So, I frantically searched all of my local stores for ANYTHING made of copper that I could use, but only managed to find some copper-plated steel measuring cups that ended up failing. Then, I used the last of my brazing wire to weld together a copper vessel of my own...which ended up getting eaten because aluminum brazing wire isn't bifluoride-resistant.
In a last-ditch effort, I tried copper plating my stainless steel reactor (the one JLCPCB sent me to sponsor this whole project), and it worked! The vessel wasn't significantly attacked when the bifluoride melted, and I was finally able to perform electrolysis. The only issue: no fluorine left the apparatus. I got a few crackles and pops from fluorine combining with stray hydrogen bubbles, but overall...nothing. I once again had red phosphorus at the outlet, which would've ignited if any fluorine was present, but it seemed to remain cold. So if fluorine was exiting the hose, it was getting sucked away by the fume hood within the first few millimeters before the phosphorus (plausible, but still disappointing). Maybe the bifluoride was wet? I doubt it, especially since some F2 was formed. Maybe it was the silicon...the electrode was coated in the thin "glassy insulating layer" described in the paper.
At this point, I just have to suck it up and publish the failure. JLCPCB needs their video! But I am majorly disappointed. This was supposed to be the epic 100K special! And besides that, I've been having SO MANY project failures...the dopamine synth, making "legal meth" (not a failure, but I did only get a tiny bit), the pound-of-thioacetone. They just keep piling up, and working in a stupidly hot garage with a hundred mosquitoes and flies doesn't help things either, lol.
Either way, it's over. At least for now. Maybe I'll buy some high-purity KHF2, pure graphite electrodes, and cast a better electrolyzer from pure copper, but it won't be for a long time. At this point, I just need to finish scripting the videos I do have and start editing and releasing them. "Making fluorine in my garage (but...)" will be first off the line, since it's sponsored, followed probably by "legal meth", then "popcorn flavor", "sodium azide from meat curing salt", and maybe my LONG overdue tellurium special (filmed LAST winter break...ouch). On my to-do list for winter break (or maybe before, if grades are good), I plan to tackle carbon tetraazide and complete the mega-thioacetone synth.
This might be my last update for a while, since college begins again on Monday, but thank you all for sticking around! Hopefully I can make this fluorine video worth your while, and provide a few more interesting videos while I'm not filming new material. Until my next update, LabCoatz out!