Admittedly, it's not quite as flawless as I had hoped for. Currently debating one more round of fit and finish. At least on the fins. The airframe tube needs a bit more paint on the fin can tube anyway.

While I'm deliberating, I can spend my time scraping the Rust-Oleum plaster that came out of my red can. Super bummed, Rust-Oleum has been awesome and reliable for me for years.

Files

Previews only

Comments

Kevin Osler

I have tried rust-Oleum over and over again with very mixed results. I read the posts about how to keep it from cracking and bubbling like that and I still seem to mess it up. I am going to try Krylon on my next rocket to see if it is operator error.

Rocket Vlogs

I've had terrible luck with Krylon. This is my first major problem with Rust-Oleum. Most cracking/lifting issues are user error in terms of prep work, re-coating too soon/too late etc. This was interesting because the color seemed to drop out and it turned clear then starting spraying huge globs of nonsense.

Emma Humphries

I’ve experienced that behavior with the last two cans of Rustoleum 2 in 1 white.